Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.33 - 1.41 g/cc | 0.0480 - 0.0509 lb/in³ | Average value: 1.38 g/cc Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Density | 1.17 - 1.41 g/cc | 0.0423 - 0.0509 lb/in³ | Average value: 1.29 g/cc Grade Count:29 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Density | 1.14 - 1.41 g/cc | 0.0412 - 0.0509 lb/in³ | Average value: 1.17 g/cc Grade Count:32 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.17 - 1.41 g/cc | 0.0423 - 0.0509 lb/in³ | Average value: 1.26 g/cc Grade Count:151 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Density | 1.17 - 1.41 g/cc | 0.0424 - 0.0509 lb/in³ | Average value: 1.26 g/cc Grade Count:22 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.38 - 1.41 g/cc | 0.0499 - 0.0509 lb/in³ | Average value: 1.39 g/cc Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | A Resin |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | OSTM059 |
Solvay TOLCIDE® PS 75 75% tetrakis hydroxymethyl phosphonium sulfate Identification: TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS).CAS: 55566 – 30 – 8Function: Industrial biocide and iron sulfide dissolverBiodegradability: BiodegradableAvailable in: .. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | OSTM059 |
Solvay BRICORR® 75 TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) Bricorr 75 contains the active ingredient tetrakishydroxylmethyl phosphonium sulphate.Identification: TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS)CAS: 55566-30-8Available in: Asia Pacific, Eur.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | OSTM059 |
Solvay TOLCIDE® PS 75LT 75% tetrakis hydroxymethyl phosphonium sulfate Identification: TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS)CAS: 55566 – 30 – 8Function: Industrial biocidal product Biodegradability: BiodegradableAvailable in: North AmericaAppli.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 81 Flexible PVC, Sheathing General purposes |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 67/K Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/4 Halogen Free PVC Sheathing, insulation; high flexibility |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/4H Halogen Free PVC Sheathing, insulation; high flexibility |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 79/R Flexible PVC, Sheathing for High Temperatures Lead Free Sheathing oil resistent |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds HL 94 Flexible PVC, Insulation for High Temperatures Operating temperature 90°C |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 0209 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 105°C |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 006 Flexible PVC, Sheathing Mineral oil resistent |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 9230 Flexible PVC, Injection Molding for Technical Items Statues |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 93 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.38 - 1.41 g/cc | 0.0499 - 0.0509 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 222 Flexible PVC, Sheathing Lead Free General purposes (80°) |
|||
Density | 1.39 - 1.41 g/cc | 0.0502 - 0.0509 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.07 - 1.41 g/cc | 0.0387 - 0.0509 lb/in³ | Average value: 1.35 g/cc Grade Count:60 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.37 - 1.41 g/cc | 0.0495 - 0.0509 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 80/R1 Flexible PVC, Lead Free Water pipes |