Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0452 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.18 - 1.25 g/cc
0.0426 - 0.0452 lb/in³
Reliance Industries METABOLIX PHB
Information provided by Reliance Industries
Density 1.07 - 1.25 g/cc
0.0388 - 0.0452 lb/in³
Average value: 1.16 g/cc Grade Count:3
Overview of materials for Polystyrene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro..
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
Apparent
Gouda Vuurvast FI 65-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Density 1.14 - 1.25 g/cc
0.0412 - 0.0452 lb/in³
253 Resin
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive
LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum..
Density 1.20 - 1.25 g/cc
0.0434 - 0.0452 lb/in³
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
FTTC 2443
Formosa Plastics 12.5% Sodium Hypochlorite
Information provided by Formosa Plastics Corporation, USA
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
Dow BETAMATE™ 7200 Polyurethane Prepolymer
BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It..
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
Dow BETAMATE™ 7201 Polyurethane Prepolymer
BETAMATE™ 7201 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It..
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds FAINGUM 7010 Flexible PVC, Injection Molding for Footwear
Soles with rubber
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds GA 006 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds GS 82/SN Flexible PVC, Injection Molding for Transparent Technical Items
Technical items high transparency
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds GSO 65/33 Flexible PVC, Injection Molding for Footwear
Soles, opaque surface
Density 1.20 - 1.25 g/cc
0.0434 - 0.0452 lb/in³
ASTM D792, ISO 1183
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber
Characteristics: 20% glass fibre filled
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1184
Fainplast Compounds MPH 75 Medical Flexible PVC, Extrusion
Tubolar apparatus
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1184
Fainplast Compounds MPH 78/H Medical Flexible PVC, Extrusion
Technical tubes no DOP
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1184
Fainplast Compounds MPH 83/T Medical Flexible PVC, Extrusion
Technical tubes no DOP
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PH 50/AL Flexible PVC, Transparent Extrusion
Food belt carriers FDA
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PH 75/C Flexible PVC, Transparent Extrusion
Profiles, UL 94 Class V1
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PH 82/A Flexible PVC, Transparent Extrusion
Transparent profiles and pipes
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PHT 0144 Flexible PVC, Transparent Extrusion
Profiles high temperatures
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1184
Fainplast Compounds KLT 93 Flexible PVC, Insulation Transparent Cables Lead Free
Transparent cables (105°C)
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds MGS 75 Medical Flexible PVC, Injection Molding
Connectors and special components
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PHA 81 Flexible PVC, Transparent Extrusion
Atoxic pipes
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PMP 75/OP Flexible PVC, Extrusion Modified with PU
High resistance to oil and hydrocarbon, with good abrasion resistance and elasticity
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
Apparent
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
Apparent
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds PMP 102 Flexible PVC, Extrusion Modified with PU
Oil resistant sheath
Density 0.950 - 1.25 g/cc
0.0343 - 0.0452 lb/in³
Average value: 1.16 g/cc Grade Count:11
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and ..
Density 1.25 - 1.25 g/cc

@Temperature 250 - 250 °C
0.0452 - 0.0452 lb/in³

@Temperature 482 - 482 °F
Average value: 1.25 g/cc Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved