Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Latrobe HS-105â„¢ ASTM M35 DIN 1.3243 High Speed Steel HS-105 high speed steel is a cobalt-modified M2 high speed steel in which the cobalt addition provides hot hardness that is intermediate between those of M2 and M42 high speed steels. The improved h.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Latrobe HS-29XLâ„¢ ASTM M2-HC High Speed Steel HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and
superior red hardness compared.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Lucas-Milhaupt Silvaloy® 5 Brazing Alloy Silvaloy 5 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Special Metals INCONEL® Alloy G-3 A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy Data provided by the manufacturer, Special Metals. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |
|||
Density | 8.15 g/cc | 0.294 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 8.15 g/cc | 0.294 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific) LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 8.15 g/cc | 0.294 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific) LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Weartech International WT-50 Nickel Hardfacing & Wear Resistant Alloy Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applicationsInformation provided by Weartech International |
|||
Density | 8.15 g/cc | 0.294 lb/in³ | |
Goodfellow Permendur 49® Cobalt Iron Magnetic Alloy Information provided by Goodfellow. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Crucible Steel Rex M2 High Speed Steel Rex M2 is a tungsten-molybdenum general purpose high speed steel. It is suitable for a wide variety of cutting tools and is often used for metalforming tools such as punches and dies. Rex M2 is a go.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2 REX M2S (1.0C) is a sulfur-bearing high carbon version of the regular CRUCIBLE REX M2 high speed steel. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Crucible Steel REX® M2 S High Speed Steel REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excell.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Carpenter Super Invar 32-5 Carpenter Super Invar 32-5, a magnetic, austenitic, solid solution alloy containing iron, nickel and cobalt, is designed to provide minimum thermal expansion at room temperatures. This alloy also e.. |
|||
Density | 8.15 g/cc | 0.294 lb/in³ | |
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100 AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal .. |
|||
Density | 8.13 g/cc | 0.294 lb/in³ | |
ATI Allegheny Ludlum AL 825™ Nickel Alloy Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing enviro.. |
|||
Density | 8.14 g/cc | 0.294 lb/in³ | |
Latrobe Double Six™ ASTM M2 High Speed Steel DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far