Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.163 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 4.50 g/cc
0.163 lb/in³
Kobe Steel KS100 Commercially Pure Titanium, Annealed
Nominal Composition: Ti-Fe-OApplications: Wrist watches, cutlery, golf club heads.Features: Scratch resistant, easy to polish, high strength. Information provided by Kobe Steel
Density 4.50 g/cc
0.163 lb/in³
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed
Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel
Density 4.51 g/cc
0.163 lb/in³
Kobe Steel KS60 Commercially Pure Titanium, ASTM Gr. 2, Annealed
Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance..
Density 4.50 g/cc
0.163 lb/in³
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed
Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant...
Density 4.51 g/cc
0.163 lb/in³
Kobe Steel KS85 Commercially Pure Titanium, ASTM Gr. 4, Annealed
Nominal Composition: Ti-Fe-OApplications: Airplane Parts.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel
Density 4.50 g/cc
0.163 lb/in³
LATI Latamid 12 H 90FE03 PA 12, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Density 4.50 g/cc
0.163 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Density 4.50 g/cc
0.163 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Density 4.50 g/cc
0.163 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT
LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Density 4.51 g/cc
0.163 lb/in³
Typical
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties
Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v..
Density 4.51 g/cc
0.163 lb/in³
Typical
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2)
Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,..
Density 4.51 g/cc
0.163 lb/in³
Typical
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy
Weldable, High Strength, High Temperature, Creep Resistant AlloyFeatures: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIME..
Density 4.51 g/cc
0.163 lb/in³
Typical
TIMET TIMETAL® Code 12 Titanium Alloy (ASTM Grade 12)
Features: Highly weldable, near-alpha alloy, exhibiting improved strength and temperature capability over CP combined with superior crevice corrosion resistance and excellent resistance under oxidiz..
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250)
Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 11 Titanium (UNS R52250)
Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252)
Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550)
Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 4 Titanium (UNS R50700)
Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.51 g/cc
0.163 lb/in³
ATI Allvac® Grade 12 UNS R53400 Titanium Alloy
Uses: Industrial components. CPI equipment, heat exchangers, pressure vessels, fittings, tubing.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided by..
Density 4.50 g/cc
0.163 lb/in³
BASF Sicotan® Yellow K 1010 Color Additive
Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B..
Density 4.50 - 5.50 g/cc
0.163 - 0.199 lb/in³
Alliance BIN-48 Bonded (Composite) Magnetic Material
Density 4.50 - 5.50 g/cc
0.163 - 0.199 lb/in³
Alliance BIN-55 Bonded (Composite) Magnetic Material
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402)
Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.51 g/cc
0.163 lb/in³
ATI Allvac® 30, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets.
Density 4.51 g/cc
0.163 lb/in³
ATI Allvac® 55, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds.
Density 4.50 g/cc
0.163 lb/in³
Ceradyne Ceralloy® 225 Titanium Diboride
Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company
Density 4.51 g/cc
0.163 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific)
LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400)
Uses: heat exchangers, industrial components, tubing, CPI equipment.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.52 g/cc
0.163 lb/in³
ATI Allegheny Ludlum Grade 7 Titanium (UNS R52400)
Uses: CPI equipment, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Density 4.50 g/cc
0.163 lb/in³
LATI Latimass 62-05 D040 PA6
Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..