Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ceradyne Ceralloy® 225 Titanium Diboride

Category Ceramic , Boride
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® 225 Titanium Diboride.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 4.50 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 2100
2100
0.3
Modulus of Elasticity 540 GPa
78300 ksi
Flexural Strength 265 MPa

@Temperature 23.0 °C
38400 psi

@Temperature 73.4 °F
Poissons Ratio 0.22
0.22
Fracture Toughness 5.47 MPa-m½
4.98 ksi-in½
Shear Modulus 221 GPa
32100 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C

@Temperature 20.0 - 1000 °C
4.56 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000100 ohm-cm
0.0000100 ohm-cm
Descriptive Properties Value Comments
Purity, % >98.5