Material Notes:
Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 345 MPa
>= 50000 psi
Tensile Strength, Yield 275 - 450 MPa

@Strain 0.200 %
39900 - 65300 psi

@Strain 0.200 %
Elongation at Break >= 20 %
>= 20 %
Reduction of Area >= 30 %
>= 30 %
Bend Radius, Minimum 2.0 t
2.0 t
t ≤ 1.8 mm
2.5 t
2.5 t
1.8 < t ≤ 4.75 mm
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti >= 99.325 %
>= 99.325 %
As Remainder