Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC (Asia Pacific) LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur.. |
|||
Density | 1.65 - 1.75 g/cc | 0.0596 - 0.0632 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead
(discontinued **) Improved Impact Strength, Low Flash, Low Warpage. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Hollow Articles Under Pressure, Pump HousingsProcessing: Injection Mo.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | |
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V9290 PET (Europe-Africa-Middle East) 45% GF PET, Glass, Mold Release, Heat Stabilized, |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | DIN 53 479 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 Method A |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Conditioned, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RVL29XXP PA 66 (Europe-Africa-Middle East) LNP VERTON* RVL29XXP is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |