LNP VERTON* RVL29XXP is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 231 MPa
33500 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ISO 527
Flexural Strength 362 MPa
52500 psi
ISO 178
Flexural Modulus 14.1 GPa
2050 ksi
ISO 178
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1A
Coefficient of Friction, Dynamic 0.39
0.39
ASTM D3702 Modified
Coefficient of Friction, Static 0.40
0.40
ASTM D3702 Modified
K (wear) Factor 42.3 x 10<sup>-8</sup> mm³/N-M
21.0 x 10<sup>-10</sup> in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 258 °C
496 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94 by SABIC-IP