Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | DIN 53479; ASTM D792 |
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Plenco 51335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L GY300 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and LubricantFeatures: Flame Retardant, Heat St.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF/M30 UV BK 30% Glass Milled/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Milled/Glass Fiber, 30% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInforma.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton UV00A PPA LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton UV00A PPA (Asia Pacific) LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Polyplastics Duranex® 7400W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |