Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183-1 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PC GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and He.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO TX10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear LNP* THERMOCOMP* OC006 is a compound based on PPS-Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Plenco 3554 Phenolic, Granular, Compression Molded PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | |
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)
(Unverified Data**) X-ray Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400XRD NC010 is a filled medium viscosity acetal copolymer for injection molding. It is detected i.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-83 Compression Molded PPS Compound, Filled with 10% PTFE, 10% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 83 Flexible PVC, Sheathing General purposes |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 91 Flexible PVC, Insulation Lead Free Power cables |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1184 |
Fainplast Compounds GSK 78 Flexible PVC, Electrical Plugs Lead Free Plugs |
|||
Density | 1.43 - 1.47 g/cc | 0.0517 - 0.0531 lb/in³ | ISO R 1183 |
Fainplast Compounds HL 88 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C, flame retardant, oil resisting |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | cured; ASTM D794 |
3M Scotchcast™ 260 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin 15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | (Dry) |
BASF Capron® 8360 HS 34% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8360 HS is a heat stabilized 34% mineral reinforced nylon 6 injection molding resin possessing a high level of toughness and ductility combined with excellent processability and surface aesth.. |
|||
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
LATI LARAMID G/30 30% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |