Ensinger Tecatron® XP-83 Compression Molded PPS Compound, Filled with 10% PTFE, 10% Graphite and 15% Carbon Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler , Polyphenylene Sulfide (PPS) with PTFE Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-83 Compression Molded PPS Compound, Filled with 10% PTFE, 10% Graphite and 15% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Filler Content 35 %
35 %
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength 35.9 MPa
5200 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 53.1 MPa
7700 psi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black