Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 2034 PC (Europe-Africa-Middle East) LEXAN 2034 is a medium viscosity flame retardant grade. The material is UV-stabilized. Glow wire at 960C also satisfies EDF spec HN 60-S-02. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermo.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | |
LATI Lastane 50 PUR Polyurethane (PUR). Unfilled. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
LyondellBasell Hostacomâ„¢ AE716BC Polypropylene Homopolymer Description: Hostacomâ„¢ AE716BC conventional melt flow, 1,400 MPa flexural modulus, UV-stabilized, 40% calcium carbonate-filled polypropylene homopolymer has a good balance of properties and pro.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM Data |
Styron CALIBRE™ SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexu.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | DIN 53479 |
Polyram RamOfin PPH353M8 Polypropylene, 40% Mineral Filled 40% mineral filled polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | DIN 53479 |
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber 15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Eurostar Staramide RF003S PA66, 15% Glass Fiber Filled, Injection Molded Staramide RF003S is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Teijin Panlite® GS-3410 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Density | 1.24 - 1.33 g/cc | 0.0448 - 0.0480 lb/in³ | Average value: 1.29 g/cc Grade Count:24 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com.. |
|||
Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |