Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® 372 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® 372 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Water Absorption 1.22 %
1.22 %
Saturation in water
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Equilibrium at 50% RH
Water Absorption at Saturation 1.22 %
1.22 %
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
DIN 53505
Elongation at Break >= 50 %
>= 50 %
Nominal
Tensile Creep Modulus, 1 hour 455 MPa
66000 psi
Tensile Creep Modulus, 1000 hours 158 MPa
22900 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C
138 °F
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
Vicat Softening Point 79.0 °C
174 °F
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
Surface Resistance 9.00e+14 ohm
9.00e+14 ohm
Dielectric Constant 3.9

@Frequency 1e+6 Hz
3.9

@Frequency 1e+6 Hz
4.6

@Frequency 100 Hz
4.6

@Frequency 100 Hz
Dielectric Strength 23.7 kV/mm
602 kV/in
Dissipation Factor 0.029

@Frequency 1e+6 Hz
0.029

@Frequency 1e+6 Hz
0.031

@Frequency 100 Hz
0.031

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V