Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.38 - 1.67 g/cc | 0.0499 - 0.0603 lb/in³ | Average value: 1.43 g/cc Grade Count:148 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.49 - 1.67 g/cc | 0.0538 - 0.0603 lb/in³ | Average value: 1.53 g/cc Grade Count:20 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Density | 1.02 - 1.67 g/cc | 0.0368 - 0.0603 lb/in³ | Average value: 1.20 g/cc Grade Count:126 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.41 - 1.67 g/cc | 0.0509 - 0.0603 lb/in³ | Average value: 1.50 g/cc Grade Count:104 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Density | 1.63 - 1.67 g/cc | 0.0589 - 0.0603 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFC 0108/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 7846Information provided by Fainplast Compounds |
|||
Density | 1.14 - 1.67 g/cc | 0.0410 - 0.0603 lb/in³ | Average value: 1.36 g/cc Grade Count:665 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Density | 1.07 - 1.67 g/cc | 0.0385 - 0.0603 lb/in³ | Average value: 1.24 g/cc Grade Count:133 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Density | 1.14 - 1.67 g/cc | 0.0412 - 0.0603 lb/in³ | Average value: 1.27 g/cc Grade Count:363 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Density | 1.33 - 1.67 g/cc | 0.0480 - 0.0603 lb/in³ | Average value: 1.45 g/cc Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |