Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.20 g/cc | 0.0426 - 0.0434 lb/in³ | ASTM D792 |
Plaskolite Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Density | 1.18 - 1.20 g/cc | 0.0426 - 0.0434 lb/in³ | ASTM D792 |
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | |
Prodways PLASTCure ABS 3650 3D Printing Polymer Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur.. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Cast 100 3D Printing Polymer High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Model 100 3D Printing Polymer Allows production of precise components; high workability.Used for dental applications from models for restorations to orthodontics.Information provided by Genistar. |
|||
Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Prodways PLASTCure Model 200 3D Printing Polymer High temperature resistance.Thermoforming applicationsInformation provided by Genistar. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Model 300 3D Printing Polymer Good mechanical properties.Broad range of dental model applications.Information provided by Genistar. |
|||
Density | 1.12 - 1.20 g/cc | 0.0405 - 0.0434 lb/in³ | Wet Density (Depending on Tamp Density) |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® T22 Tamping Mix Description: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is a wet taping mix made up of bulk refractory fibers and a high temperature binder system. T22 FIBERPAK® TAMPING MIX is particularly good.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8510 TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8510H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8510L TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8511H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 60/AS Flexible PVC, Injection Molding for Footwear Oil resistent and antistatic soles |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 75/R1 Flexible PVC, Injection Molding for Footwear Soles antiaccident shoes |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds FAINGUM 6530 Flexible PVC, Injection Molding for Footwear Soles with rubber |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 62/T Medical Flexible PVC, Extrusion Technical tubes and peristaltic pump segments no DOP |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 572D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 001/14 Flexible PVC, Extrusion Modified with PU Various profiles |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds POLIFAIN 6020 Flexible PVC, Injection Molding for Footwear Soles with PU |
|||
Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 0.920 - 1.20 g/cc | 0.0332 - 0.0434 lb/in³ | Average value: 0.987 g/cc Grade Count:123 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Density | 1.10 - 1.20 g/cc @Temperature 285 - 285 °C |
0.0397 - 0.0434 lb/in³ @Temperature 545 - 545 °F |
Average value: 1.19 g/cc Grade Count:27 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Density | 0.950 - 1.20 g/cc | 0.0343 - 0.0434 lb/in³ | Average value: 1.13 g/cc Grade Count:94 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Density | 0.970 - 1.20 g/cc | 0.0350 - 0.0434 lb/in³ | Average value: 1.12 g/cc Grade Count:8 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |