Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 - 1.17 g/cc | 0.0415 - 0.0423 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.16 - 1.17 g/cc | 0.0419 - 0.0423 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet TangoGray FullCure950 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.03 - 1.17 g/cc @Temperature 250 - 250 °C |
0.0372 - 0.0423 lb/in³ @Temperature 482 - 482 °F |
Average value: 1.10 g/cc Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 0.940 - 1.17 g/cc | 0.0340 - 0.0423 lb/in³ | Average value: 1.03 g/cc Grade Count:41 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Density | 1.07 - 1.17 g/cc | 0.0387 - 0.0423 lb/in³ | Average value: 1.11 g/cc Grade Count:4 |
Overview of materials for Nylon 11 with Graphite Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.05 - 1.17 g/cc | 0.0379 - 0.0423 lb/in³ | Average value: 1.07 g/cc Grade Count:7 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.125 - 1.17 g/cc | 0.04064 - 0.0423 lb/in³ | OSTM059 |
Solvay AQUARITE® ESL Surfactant Identification: PHOSPHONATE END CAPPED SULPHONATED COPOLYMERAvailable in: Asia Pacific, Europe, Latin America and North America. Applications: AQUARITE® ESL is a patented, high performance, broad.. |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 39/T Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 46/T Flexible PVC, Injection Molding for Footwear Vamp boots |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 65/R-AS Flexible PVC, Injection Molding for Footwear Oil resistent and antistatic soles |
|||
Density | 1.15 - 1.17 g/cc | 0.0416 - 0.0423 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 50/T Medical Flexible PVC, Extrusion Technical tubes and peristaltic pump segments no DOP |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 45/1 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | Internal |
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Density | 1.13 - 1.17 g/cc | 0.0408 - 0.0423 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 590A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.15 - 1.17 g/cc | 0.0415 - 0.0423 lb/in³ | |
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, in.. |
|||
Density | 1.15 - 1.17 g/cc | 0.0415 - 0.0423 lb/in³ | |
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane AdvanSource Biomaterials Corporation manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with .. |
|||
Density | 0.679 - 1.17 g/cc | 0.0245 - 0.0423 lb/in³ | Average value: 1.14 g/cc Grade Count:63 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Density | 1.08 - 1.17 g/cc | 0.0390 - 0.0423 lb/in³ | Average value: 1.13 g/cc Grade Count:13 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.01 - 1.17 g/cc | 0.0365 - 0.0423 lb/in³ | Average value: 1.13 g/cc Grade Count:64 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |