Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | RT |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Piezo Kinetics 556 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Indium Corp. Indalloy® 209 Sn-Ag-Sb Solder Alloy Low temperature die attach alloy. Has very high tensile strength. Old Motorola die attach solder; very brittle.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel Superplast® 400 High Hardness Mold Steel SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (496°C - 4 hours + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corr.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corr.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (496°C - 4 hours - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy Applications: pump sleevesInformation provided by Weartech International |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Crucible Steel CPM® 3V® Tool Steel CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact to.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 925 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | Typical |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | Typical |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 925 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.80 - 8.00 g/cc | 0.282 - 0.289 lb/in³ | |
PSM Industries Pacific Sintered Metals Yellow Brass BZ-111-UC Powdered Metal 80-20 leaded brass, Coined for close dimensional control, strength and density Equivalent MPIF Specification: CZP-2000-12Information Provided by Pacific Sintered Metals, a division of PSM Industrie.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | |
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |
|||
Density | 7.80 g/cc | 0.282 lb/in³ | Estimated by MatWeb |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |