Crucible Steel CPM® 3V® Tool Steel

Category Metal , Ferrous Metal , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® 3V® Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact toughness greater than A2, D2, Cru-Wear or CPM M4, approaching the levels of S7 and other shock resistant grades, while providing excellent wear resistance, high hardness and thermal stability for coatings. Intended to be used at HRC 58-60 CPM 3V can replace high alloy tool steels in wear applications where chronic tool breakage and chipping problems are encountered. The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 241
241
Annealed
Hardness, Rockwell C 58 - 60
58 - 60
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 53.0 J
39.1 ft-lb
Austenitizing Temperature- 1120°C
95.0 J
70.1 ft-lb
Austenitizing Temperature- 1065°C
113 J
83.3 ft-lb
Austenitizing Temperature- 1025°C
Thermal Properties Metric English Comments
CTE, linear 10.6 µm/m-°C

@Temperature 20.0 - 200 °C
5.89 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 24.2 W/m-K

@Temperature 200 °C
168 BTU-in/hr-ft²-°F

@Temperature 392 °F
Component Elements Properties Metric English Comments
Carbon, C 0.80 %
0.80 %
Chromium, Cr 7.5 %
7.5 %
Iron, Fe 88.65 %
88.65 %
As Remainder
Molybdenum, Mo 1.3 %
1.3 %
Vanadium, V 2.75 %
2.75 %