Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Piezo Kinetics 556 Lead Zirconate Titanate Piezoelectric

Category Ceramic , Oxide , Titanium Oxide , Zirconium Oxide , Piezoelectric
Manufacturer Piezo Kinetics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Piezo Kinetics 556 Lead Zirconate Titanate Piezoelectric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 value, higher k33 , and lower loss factor. This formulation aids the design engineer by giving more flexibility within the type VI class of materials.Elastic Compliance s11E (x 10-12 m²/n): 13.8.Elastic Compliance s33E (x 10-12 m²/n): 17.2.Property data at 25°C. Information supplied by Piezo Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 58.0 GPa
8410 ksi
Poissons Ratio 0.22
0.22
Shear Modulus 24.0 GPa
3480 ksi
calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Maximum Operating Temperature
Electrical Properties Metric English Comments
Curie Temperature 180 °C
356 °F
Dielectric Constant 3900

@Frequency 1000 Hz
3900

@Frequency 1000 Hz
Dissipation Factor 0.022

@Frequency 1000 Hz
0.022

@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.75
0.75
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -310
-310
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 750
750
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 17.4
17.4
Piezoelectric Planar Coupling Factor, kp 0.67
0.67
Piezoelectric Mechanical Q 65
65
Piezoelectric Shear Coupling Factor, k15 0.68
0.68
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 600
600
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -9.00
-9.00
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 21.7
21.7
Piezoelectric Transverse Coupling Factor, k31 0.40
0.40