Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.90 - 1.95 g/cc | 0.0686 - 0.0704 lb/in³ | |
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | True Density |
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber
(discontinued **) Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
IDI Composites W-103 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52615 Injection Molding CPP. 70% CaCO3FilledWhite UV Stable.Information provided by Multibase |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |
|||
Density | 1.90 g/cc @Thickness >=0.000 mm |
0.0686 lb/in³ @Thickness >=0.000 in |
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Applied Composites 8092 Polyester SMC Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo.. |
|||
Density | 1.90 - 2.20 g/cc | 0.0686 - 0.0795 lb/in³ | |
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only) Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Inj.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTABIO EX 03120 B Biodegradable Plastic, Calcium Carbonate Filled Blend of fine calcium carbonate and BASF ECOFLEX™Certified for food contactInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® W800 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |