Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity .. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
3M Dyneon™ Fluorel™ FE-5642Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
IDI Composites C-105 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D572 |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
SGL Carbon Group EK 2239 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S012 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4433 Compressed Inorganic Fiber Sheet Fiberglass, Aramid & Inorganic FibersNitrile BinderUltimate Steam SheetOutstanding Load BearingExcellent Creep RelaxationBest General Purpose SheetInformation provided by Thermoseal Inc. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Washington Penn PPH5CF75 Polypropylene, 75% Calcium Carbonate Filled Concentrate UV Stabilized.Applications: ShelvingData provided by Washington Penn Plastic Co., Inc. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Cured |
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Cured |
Chesterton MRS SD4i Metal Rebuilding System An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shri.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-63 Compression Molded PPS Compound, 50% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
Epoxyset Epoxibond EB-315 Low Expansion Epoxy Adhesive EB-315 is a highly filled, heat curing, high temperature resistant epoxy adhesive. Due to its low coefficient of thermal expansion and outgassing, it can be used for bonding and sealing in critical .. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Applied Composites 8007 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Pigmentable, Low Water Absorption, Weathering Resistant, Good Corrosion Resistance in Waste Water Environment.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
Parkway Products Thixomolded® AZ91D Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | Molded |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther.. |