Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Thermoseal KLINGERSIL® C-4433 Compressed Inorganic Fiber Sheet

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Thermoseal Inc.
Trade Name KLINGERSIL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal KLINGERSIL® C-4433 Compressed Inorganic Fiber Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiberglass, Aramid & Inorganic FibersNitrile BinderUltimate Steam SheetOutstanding Load BearingExcellent Creep RelaxationBest General Purpose SheetInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM F1315
Thickness 1588 microns
62.52 mil
Thickness tested
Electrical Properties Metric English Comments
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149-95a
Descriptive Properties Value Comments
Color Red
(Top/Bottom)
Compressibility 7 percent
ASTM F36J
Creep Relaxation 20 percent
1/32", ASTM F38B
Gas Permeability <0.2 ml/min
DIN 3535/6
Klinger Hot Compression Test 7 percent
Initial, Thickness Decrease 73°F (23°C)
8 percent
Additional, Thickness Decrease 572°F (300°C)
Leachable Chloride Content 150 ppm
FSA Method (Typical)
Recovery >60 percent
ASTM F36J
Sealability <0.5 ml/hr
1/32", ASTM F37A
Thickness Increase 0-4%
ASTM Oil IRM903, 5h/300°F (149°C)
0-5%
ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
0-5%
ASTM Fuel A, 5h/73°F (23°C)
0-7%
ASTM Fuel B, 5h/73°F (23°C)
Weight Increase <10%
ASTM F146 after immersion in Fuel B 5h/73°F (23°C)