| Category | Metal , Nonferrous Metal , Magnesium Alloy |
| Manufacturer | Parkway Products |
| Trade Name | Thixomolded® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Parkway Products Thixomolded® AZ91D Magnesium.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.80 g/cc | 0.0650 lb/in³ | |
| Porosity | 0.0 - 1.1 % | 0.0 - 1.1 % | |
| 0.0 - 1.10 % | 0.0 - 1.10 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell E | 75 | 75 | |
| Tensile Strength, Ultimate | 248 MPa | 36000 psi | |
| Tensile Strength, Yield | 159 MPa | 23000 psi | |
| Elongation at Break | 6.0 % | 6.0 % | |
| Modulus of Elasticity | 44.8 GPa | 6500 ksi | |
| Poissons Ratio | 0.35 | 0.35 | |
| Shear Modulus | 17.0 GPa | 2470 ksi | calculated |
| Impact Test | 4.75 J | 3.50 ft-lb |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 24.8 µm/m-°C @Temperature 21.1 °C |
13.8 µin/in-°F @Temperature 70.0 °F |
|
| Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
| Thermal Conductivity | 72.0 W/m-K | 500 BTU-in/hr-ft²-°F | |
| Melting Point | 596.1 °C | 1105 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | >= 371 °C | >= 700 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Aluminum, Al | 8.3 - 9.7 % | 8.3 - 9.7 % | |
| Copper, Cu | <= 0.030 % | <= 0.030 % | |
| Iron, Fe | <= 0.0050 % | <= 0.0050 % | |
| Magnesium, Mg | 90 % | 90 % | As Remainder |
| Manganese, Mn | >= 0.13 % | >= 0.13 % | |
| Nickel, Ni | <= 0.0020 % | <= 0.0020 % | |
| Silicon, Si | <= 0.10 % | <= 0.10 % | |
| Zinc, Zn | 0.35 - 1.0 % | 0.35 - 1.0 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000140 ohm-cm | 0.0000140 ohm-cm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Across Parting Line Dimensions | + 0.0015 in | Tolerance (0 - 10 in<sup>2</sup>) |
| + 0.0025 in | Tolerance (11 - 20 in<sup>2</sup>) | |
| + 0.004 in | Tolerance (21 - 50 in<sup>2</sup>) | |
| + 0.006 in | Tolerance (51 - 100 in<sup>2</sup>) | |
| Flatness Across Largest Dimension | +/- 0.001 in | Tolerance (each inch beyond 1 in) |
| +/- 0.002 in | Tolerance (0 - 3 in) | |
| Ignition Temperature at One Atmosphere | >900°F | |
| Linear Dimension in same Die Half | +/- 0.0005 in | Tolerance (0 to 1 in) |
| +/- 0.0010 in | Tolerance (each inch beyond 1 in) | |
| Mil 117B Salt Spray Corrosion | 2.8 Mils per Year | |
| Moving Die Component Tolerances | + 0.004 in | Tolerance (0 - 10 in<sup>2</sup>) |
| + 0.006 in | Tolerance (11 - 20 in<sup>2</sup>) | |
| + 0.008 in | Tolerance (21 - 50 in<sup>2</sup>) | |
| + 0.010 in | Tolerance (51 - 100 in<sup>2</sup>) | |
| Shielding Effectiveness 0.020" thk | >85 dB | 100MHz |
| Shielding Effectiveness 0.050" thk | >88 dB | 100MHz |
| Surface Finish | 32 RMS or better | |
| Thickness | 0.015 - 2.0 in | |
| UL94 Flame Exposure Results | DNB |