Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO.1183 DIN.53479 |
Omnia Plastica PVDF Kynar PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | Solid |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183-1 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL24 PVDF LNP* Lubricomp* 5CL24 is a compound based on Polyvinylidene Fluoride resin containing 10% PTFE and 20% Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1010/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1015/1001 Polyvinylidene Fluoride
(discontinued **) Ultra-high molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabil.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 0177 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-400 1K HTA-7W EP01 Continuous Filament Carbon Fiber Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-500 3K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.12000 filaments/strand.Thornel® products were sold by Amoco and are now owned by Cytec. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
CENTROPLAST CENTROFLON Polyvinylidene fluoride This material has very good chemical and temperature resistance, with good slip characteristics. Its applications include pump wheels, flanges, valve bodies, and laboratory equipment.Information pr.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |