Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Kynar® 2850 PVDF Copolymer

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Westlake Plastics
Trade Name KYNAR®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Westlake Plastics Kynar® 2850 PVDF Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stable, mechanically tough, abrasion and flame resistant.Kynar® is a trade name of Elf Atochem North America. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Tensile Modulus 0.862 GPa
125 ksi
ASTM D638
Flexural Yield Strength 46.9 MPa
6800 psi
ASTM D790
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
78.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 157 °C
315 °F
ASTM D4591
Maximum Service Temperature, Air 116 °C
240 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
ASTM D648
Flammability, UL94 V-0
V-0
Oxygen Index 42 %
42 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 7.5

@Frequency 1000 Hz
7.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 10.6 kV/mm
270 kV/in
ASTM D149