Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvents, and oxidizing environments. It also has outstanding aging resistance, with its properties remaining constant after many years of continuous use.Uses: ENSIKEM's excellent chemical and physical properties and the ease with which it can be processed make it especially suitable for components in the chemical, petrochemical, hydrometallurgical, pharmaceutical, food, nuclear, and paper and pulp industries, as well as the semiconductor processing industry. Information supplied by Ensinger, Inc.Ensikem grades have been replaced by Tecaflon
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption <= 0.040 %
<= 0.040 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Ultimate 53.4 MPa
7750 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Modulus of Elasticity 2.40 GPa
348 ksi
1% Secant; ASTM D638
Flexural Yield Strength 74.1 MPa
10700 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
Tangent; ASTM D790
Compressive Yield Strength 80.0 MPa
11600 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 128 µm/m-°C

@Temperature 20.0 °C
71.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 178 °C
352 °F
ASTM D3448
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 113 °C
235 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Dielectric Constant 9.0

@Frequency 60 Hz
9.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.0 kV/mm
280 kV/in
ASTM D149
Dissipation Factor 0.060

@Frequency 60 Hz
0.060

@Frequency 60 Hz
ASTM D150
Users viewing this material also viewed the following: