Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific) LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA4/6 GF50 HS BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackUL File Number: E1573.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT LNP* THERMOCOMP* WF006H is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS2 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGF25/25 22H-NBK1 Nylon 66, 25% Mineral and 25% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® 46HF4550 PA46-GF50 50% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLOW HF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection PBT-MD30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
BASF Ultramid® 8232G HS FR BK-102 25% Glass Filled PA6 (Dry) Ultramid 8232G HS FR BK-102 is a 25% glass fiber reinforced, heat stabilized, flame retardant pigmented black PA6 injection molding compound exhibiting excellent melt stability characteristics. It .. |
|||
Density | 1.62 g/cc @Temperature 23.0 °C |
0.0585 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
DSM Arnite® TV6 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |