| Category | Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled |
| Manufacturer | Barlog Plastics |
| Trade Name | KEBAFLOW |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Barlog Plastics KEBAFLOW HF130 LCP, 30% glass fiber reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
| Water Absorption | 0.040 % | 0.040 % | similar to ISO 62 test |
| Linear Mold Shrinkage, Flow | 0.0016 cm/cm | 0.0016 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0046 cm/cm | 0.0046 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 136 MPa | 19700 psi | ISO 527-1 |
| Elongation at Break | 1.5 % | 1.5 % | ISO 527-1 |
| Tensile Modulus | 14.0 GPa | 2030 ksi | ISO 527-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 305 °C | 581 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
UL Registered; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Resin Type | LCP-GF30 |