Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
PolyOne OnForce™ LFT AM-40LGF/001 Natural Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | molded; ISO 1183 |
SABIC Innovative Plastics Cycolac® INP449 SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agentThis data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES Plaslube® J-50/30/TF/10 Polycarbonate, 30% GFR, 10% PTFE Plaslube glass fiber reinforced polytetrafluorethylene (PTFE) lubricated polycarbonate grades have an excellent balance of mechanical strength characteristics, dimensional stability and wear and fri.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66 LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Density | 1.53 - 1.55 g/cc | 0.0553 - 0.0560 lb/in³ | Laminate |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Nominal Laminate |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/48370/1000 Fiber: HR 12K, 2x2 Twill, 370 g/m2Information provided by HexCel |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | dry; ISO 1183 |
DSM Stanyl® SC50 PA46-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 019/G Halogen Free PVC Sheathing; high flexibility |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183/A |
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | |
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® MN301-G30 Nylon 66 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |