Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific) Extem XH2315 Resin |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Stir SpA AF 70 R (PVC) Application: Flame resistant sheath CEI 20-11 type TM 1Information provided by STIR SpA |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific) LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific) LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
DSM Arnite® TV8 260 PBT-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 80 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 87/1 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 215 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flame retardancy, improved processabilityInformation provided by Fainplast Compound.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | cured 14 days @ 50% RH |
3M AC-730 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | Liquid |
3M Novec™ 71IPA Engineered Fluid 3M™ Novec™ 71IPA Engineered Fluid is ideal for light cleaning and degreasing tasks. 3M™ Novec™ 71IPA has essentially constant vapor and liquid composition at its boiling point. Excellent replace.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |