Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.51 g/cc | 0.0546 lb/in³ | Crystalline; ISO 1183 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Plenco 4759 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East) LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive . |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 (Asia Pacific) LNP* Lubricomp* PFL36 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RFN18SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
Stir SpA AF 80 3 GEC (PVC) Application: Insulation CEI 20-11 type TI 1 low acid fumes emissionInformation provided by STIR SpA |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Asia Pacific) LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Plenco 4301 Phenolic, Granular, Injection Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Density | 1.51 g/cc @Temperature 23.0 °C |
0.0546 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-88 Compression Molded PPS Compound, with 10% Graphite, 15% PTFE and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | Dry as molded |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON KEL32 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL32 is a compound based on Acetal Copolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Density | 1.51 - 1.71 g/cc | 0.0546 - 0.0618 lb/in³ | Molded |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |