Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D1475 |
BASF Master Builders Solutions ChemRex® CX-26 Isocyanate-Free Polyurethane-Based Sealant
(discontinued **)< CX-26 is a polyurethane based one-component, moisture curing sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/eliminate.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock UV resistant |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPA® KN133G50 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES (Europe-Africa-Middle East) LNP* Lubricomp* JX91198 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF33 TL15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Density | 1.50 - 1.65 g/cc | 0.0542 - 0.0596 lb/in³ | |
Goodfellow Carbon/Vinyl Ester Rod Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Plenco 6301 Phenolic, Granular, Injection Molded PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183A |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 75 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | cured 14 days @ 50% RH; AMS3265 |
3M AC-730 Class C-4 (168) Aerospace Sealant 3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
3M Scotchkote™ 162CR Epoxy Coating 3M Scotchkote Epoxy Coating 162CR has been specifically developed as a 100% solids lining for eth internals of tanks, vessels and other equipment in contact with dirty water, mild aqueous chemicals .. |
|||
Density | 1.50 g/cc @Temperature 23.0 °C |
0.0542 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Conditioned) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G20F PBT Resin 20% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 32 Halogen Free PVC General purpose |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |