Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Master Builders Solutions ChemRex® CX-26 Isocyanate-Free Polyurethane-Based Sealant  (discontinued **)<

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Master Builders Solutions ChemRex® CX-26 Isocyanate-Free Polyurethane-Based Sealant  (discontinued **)<.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CX-26 is a polyurethane based one-component, moisture curing sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/eliminate mechanical fasteners.Typical applications of CX-26 include sealing of interior/exterior joints, waterproofing overlap seams, bonding or sealing side post, and sealing compartment doors.Tack-free time is 17 minutes ± 2 minutes given the ASTM C 679 test method. Sag resistance is excellent given the ASTM C 639 test method. The tear strength is 32 pits ± 5 pits given the ASTM D 1044 test method. Adhesion-in peel is 39 pli ± 5 pli given the ASTM C 794 test method. The mandrel bend showed no cracking given the ASTM C 793 test method. Bond durability on glass, aluminum, and concrete is 12.5 % given the ASTM C 719 test method.Information provided by ChemRex, Inc.Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D1475
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
ASTM C661
Tensile Strength, Ultimate 1.42 - 1.76 MPa
206 - 255 psi
ASTM D412
Elongation at Break 288 - 288 %
288 - 288 %
ASTM D412
100% Modulus 0.000810 GPa
0.117 ksi
ASTM D412
Tear Strength Test 32
32
pit per ASTM D 1044
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Users viewing this material also viewed the following: