Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0459 lb/in³ | |
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Density | 1.27 g/cc | 0.0457 lb/in³ | Fired Density at 2000°F |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M100 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Techmer ES HiFill® HDPE E GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Techmer ES HiFill® PEI BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | dry; ISO 1183 |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183B |
Styron CALIBREâ„¢ 7101-8 Polycarbonate CALIBREâ„¢ 7101-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® S1220 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer .. |
|||
Density | 1.27 - 1.31 g/cc | 0.0459 - 0.0473 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 90/T Flexible PVC, Injection Molding for Footwear Technical items for footwear |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.27 - 1.31 g/cc | 0.0459 - 0.0473 lb/in³ | ISO R 1183 |
Fainplast Compounds GSK 74/UV Flexible PVC, Injection Molding, Lead Free Technical items for outdoor |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D 792 |
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | dry; ISO 1183 |
DSM Novamid® 3010CF30 BK PA66-CF30 30% Carbon Reinforced |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |