Thermal Properties Metric English Comments
Thermal Conductivity 0.340 W/m-K

@Temperature 600 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Pyrotek ISOMAG® 175 Structural Insulation Board
Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr..
Thermal Conductivity 0.340 W/m-K

@Temperature 100 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC503 PTFE, 15% Mineral Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon.
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 100 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 1000 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GI 26 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.340 W/m-K

@Temperature 1370 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Zircar Ceramics APA-3 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo..
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 600 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 200 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 35-12 Insulating Refractory Brick