Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 1.40 kN/m | >= 7.99 pli | ASTM D264-91 Die C |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Tear Strength | 1.40 kN/m | 8.00 pli | Initial Tear Strength |
Saint-Gobain CHR® 2355-2 FEP Film Backing Silicone Adhesive Pressure Sensitive Tape Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit.. |
|||
Tear Strength | 1.40 kN/m | 8.00 pli | Initial Tear Strength |
Saint-Gobain CHR® C Film Backing Silicone Adhesive Pressure Sensitive Tape Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit.. |
|||
Tear Strength | 1.40 kN/m | 8.00 pli | Parallel to Thickness, width |
Zircar Ceramics APA-3 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo.. |
|||
Tear Strength | 1.40 kN/m | 8.00 pli | |
Dow Corning SILASTIC® HV 1666/65 GRAY SILICONE RUBBER 65 Durometer, gray, peroxide cure, high voltage grade Silicone Rubber Compound for manufacturing High Voltage insulators weather shed insulators or surge arrestors. Superior wet electrical propertie.. |