Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 10.91 g/cc
0.3941 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.66 MPa
5317 psi
Thermal Properties Metric English Comments
CTE, linear 22.4 µm/m-°C

@Temperature 20.0 °C
12.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 33.0 W/m-K
229 BTU-in/hr-ft²-°F
Melting Point 268 - 286 °C
514 - 547 °F
Solidus 268 °C
514 °F
Liquidus 286 °C
547 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 8.0 %
8.0 %
Indium, In 1.0 %
1.0 %
Lead, Pb 86 %
86 %
Silver, Ag 1.0 %
1.0 %
Tin, Sn 4.0 %
4.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00003071 ohm-cm
0.00003071 ohm-cm
Copyright © lookpolymers.com All Rights Reserved