Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 33.0 W/m-K @Temperature 85.0 °C |
229 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not r.. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | Perpendicular to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | Perpendicular to pressing direction |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS145 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS221 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS286 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 95.0 °C |
229 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1300 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 399 °C |
229 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 599 °C |
229 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Thermal Conductivity | 33.0 W/m-K | 229 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |