Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 9.39 g/cc
0.339 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
Thermal Properties Metric English Comments
CTE, linear 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 41.0 W/m-K
285 BTU-in/hr-ft²-°F
Melting Point 185 - 243 °C
365 - 469 °F
Solidus 185 °C
365 °F
Liquidus 243 °C
469 °F
Component Elements Properties Metric English Comments
Indium, In 1.8 %
1.8 %
Lead, Pb 63.2 %
63.2 %
Tin, Sn 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001811 ohm-cm
0.00001811 ohm-cm