Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.39 g/cc | 0.339 lb/in³ | |
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.39 g/cc | 0.339 lb/in³ | |
Indium Corp. Indalloy 134 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.39 g/cc | 0.339 lb/in³ | |
Williams Advanced Alloys WS243 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 9.38 g/cc | 0.339 lb/in³ | |
AIM 70 Fusible Alloy Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seal.. |
|||
Density | 9.37 g/cc | 0.339 lb/in³ | |
Indium Corp. Indalloy 46 Bismuth Solder Alloy Information Provided by Indium Corporation |