Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 32.2 MPa
4670 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 22.0 W/m-K
153 BTU-in/hr-ft²-°F
Melting Point 184 - 209 °C
363 - 408 °F
Solidus 184 °C
363 °F
Liquidus 209 °C
408 °F
Component Elements Properties Metric English Comments
Indium, In 50 %
50 %
Lead, Pb 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002867 ohm-cm
0.00002867 ohm-cm