Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.0 W/m-K @Temperature 85.0 °C |
153 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 7 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Momentive Performance Materials Tantalum Carbide (TaC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | DIN EN 821: part 2; Laserflash |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS209 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Goodfellow Manganin® Copper Resistance Alloy Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-25 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-25 4K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 38 Copper Alloy Description: Niclal 38 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 42 Copper Alloy Description: Niclal 42 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 48 Copper Alloy Description: Niclal 48 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Thermal Conductivity | 22.0 W/m-K @Temperature 20.0 - 100 °C |
153 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EA95 Sintered Alumina, 95% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | |
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4) EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist.. |
|||
Thermal Conductivity | 22.0 W/m-K | 153 BTU-in/hr-ft²-°F | HOT-DISK; 60x60x3 mm |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |