Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.86 g/cc | 0.320 lb/in³ | |
Indium Corp. Indalloy® 7 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, weld metal as welded Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Density | 8.85 g/cc | 0.320 lb/in³ | |
Indium Corp. Indalloy 119 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Special Metals Nickel 212 Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Williams Advanced Alloys WS212 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 210 Gilding Metal, Extra Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 511 Phosphor Bronzes 4%, Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 7026 Copper Nickel, Annealed 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 70265 XP175, 1/2 Hard Information provided by Eagle Brass Company |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TD02 1/2 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TM06 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TX00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TM00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Ametek AM 388™ Alloy (UNS C72650) TM08 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Density | 8.87 g/cc | 0.320 lb/in³ | |
Indium Corp. Indalloy 208 Copper Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.86 g/cc | 0.320 lb/in³ | |
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |