Material Notes:
Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance.Applications: films, disposable gloves, tubing and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D1505
Methyl Acrylate Content 24 %
24 %
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 37
37
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 835 %
835 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 77.0 °C
171 °F
by DSC; ASTM D3418
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Blown Film
Extrusion
Film
Region US & Canada
Bamberger Polymers Distribution