Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.74 g/micron | 95.0 g/mil | ASTM D1709 |
Huntsman PE1155 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA Copolymer and FDA compliant.Features: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications:.. |
|||
Dart Drop | 3.74 g/micron | 95.0 g/mil | ASTM D1709 |
Westlake EF608 Low Density Polyethylene Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
Dart Drop | 3.74 g/micron | 95.0 g/mil | ASTM D1709 |
Westlake EF677 Low Density Polyethylene Westlake EF677 is a high melt index LDPE resin suggested for garment films, or other applications requiring excellent drawdown. This material is also an excellent choice for PE foam applications.App.. |
|||
Dart Drop | 3.74 g/micron | 95.0 g/mil | ASTM D1709 |
Westlake EF706 Low Density Polyethylene Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
Dart Drop | 3.74 g/micron | 95.0 g/mil | ASTM D1709 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |