Material Notes:
Description: High Impact Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm
0.025 - 0.030 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.020 - 0.025 cm/cm
0.020 - 0.025 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-93
Elongation at Break 140 %
140 %
ISO 527-93
Flexural Strength 55.0 MPa
7980 psi
ISO 178-93
Flexural Modulus 1.45 GPa
210 ksi
ISO 178-93
Izod Impact, Notched (ISO) 90.0 kJ/m²
42.8 ft-lb/in²
ISO 180-93
22.0 kJ/m²

@Temperature -40.0 °C
10.5 ft-lb/in²

@Temperature -40.0 °F
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93