Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® XT1627-WBK2 High Impact, Weatherable Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® XT1627-WBK2 High Impact, Weatherable Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Impact, Weatherable Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm
0.020 - 0.024 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-93
Elongation at Break 80 %
80 %
ISO 527-93
Flexural Strength 60.0 MPa
8700 psi
ISO 178-93
Flexural Modulus 1.70 GPa
247 ksi
ISO 178-93
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO 75-93
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93