Wellman Wellamid® GF33-66 22LH-N 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF33-66 22LH-N 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data provided by the manufacturer, Wellman Inc.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 1.25 %
1.25 %
Approximate 24 hr.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 190 MPa
27600 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Yield Strength 280 MPa
40600 psi
ISO 178
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.790 mm
HB

@Thickness 0.0311 in