Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM data at 5 mm/min. |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM D638 |
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM D638 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | |
GBC Grade 92 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Tensile Strength, Ultimate | 190 MPa @Temperature 980 °C |
27600 psi @Temperature 1800 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM D638 |
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
Wellman Wellamid® GF33-66 22LH-N 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ISO 527 |
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | dry; ISO 527-1/-2 |
DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | dry; ISO 527-1/-2 |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | dry; ISO 527-1/-2 |
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30 30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ATSM D638 |
Ashley Polymers Ashlene® 528L-33G Nylon 66, 33% Glass Reinforced General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ATSM D638 |
Ashley Polymers Ashlene® 528LS-33GB Nylon 66, Glass Reinforced General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | 5mm/min; ISO 527 |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | 5mm/min; ISO 527 |
BASF Ultramid® A3EG7 BK00564 35% Glass Filled PA66 (Dry) Ultramid A3EG6 BK00564 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | 5mm/min; ISO 527 |
BASF Ultramid® A3EG7 BK23189 35% Glass Filled PA66 (Dry) Ultramid A3EG6 BK23189 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | 5mm/min; ISO 527 |
BASF Ultramid® SEG8 BK-126 40% Glass Filled PA6 (Dry) Ultramid SEG8 BK-126 is a 40% glass reinforced, pigmented black, injection molding type 6 nylon requiring high strength, surface aesthetics, and good processability. This product has excellent surf.. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | Same value from ASTM and ISO tests; 5 mm/min. |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM data at 5 mm/min. |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |