Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Solventless Electrical Varnish
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Von Roll Isola USA.Flash Point: 29°C. Average solids: 48%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, and bare copper coils.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Viscosity 250 cP
250 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Electrical Properties Metric English Comments
Dielectric Strength 122 kV/mm
3100 kV/in
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Suggested baking time at this temperature is 1-4 hr.